How to Fix Blobs and Zits on 3D Prints
Contents
You take a part off the plate and the shape is right, but the outer wall has little bumps, a vertical line down one side, or a blob at a corner. These flaws are called zits or blobs, and the line is the Z seam. They rarely make a part weaker, but they are easy to see, especially on smooth, round or glossy prints.
The good news is that blobs and zits come from a short list of causes, and you can fix most of them with settings you already have in your slicer.
What blobs, zits and the seam look like
- A vertical line or row of small bumps on one side of a round part. This is the Z seam.
- Scattered tiny bumps on flat walls, often where the nozzle stopped to retract or started again.
- A blob at a sharp corner, where the plastic bulges because the nozzle slowed down while pressure was still pushing plastic out.
- A thin, weak start to a line right after a corner or a travel move.
- Bubbles, popping sounds and fuzzy bumps all over the surface, which point to wet filament rather than a settings problem.
It helps to look at where the flaw sits. A bump that always lines up in one column is the seam. Bumps spread around the wall belong to retraction or travel moves. Bumps everywhere, together with a rough texture, usually mean moisture or too much flow.
Why they happen
A printer lays down each wall as a closed loop. The loop has to start and end somewhere, and that point leaves a small mark. Stack that mark layer after layer and you get a line, which is the Z seam.
Zits have two further sources. The first is pressure in the nozzle. Melted plastic is under pressure inside the nozzle, and that pressure does not follow the print head's speed changes right away. When the head slows into a corner, plastic keeps coming out and the corner bulges. When the head speeds up on a straight, the line can start thin. The second is retraction and restarts. When the nozzle stops and pulls the filament back, a tiny amount of plastic can ooze out, and the restart can leave a small bump on a visible wall.
Hot plastic oozes more, and wet filament makes everything worse, so temperature and moisture matter too.
1. Choose where the seam goes
Every slicer lets you pick a seam position. The aim is to put the seam where nobody will look, or where it blends in.
- Aligned or Rear puts every seam in one column at the back of the part. You get a single clean line that you can turn away from the viewer. This is the most useful setting for most prints.
- Nearest or sharpest corner hides the seam in an existing corner. It works well on boxy parts, where a bump in the corner is hard to notice.
- Random scatters the seam around the part. That avoids a line, but it spreads small bumps across smooth walls, so it often looks worse on round parts.
Newer slicers also offer scarf seams, which start and end the wall with a gradual ramp so the join is much harder to see. According to the PrintPal wiki, scarf seams are available in OrcaSlicer 2.0 and later, Bambu Studio 1.9 and later and PrusaSlicer 2.9 and later, and as an experimental option in Cura 5.9. If your slicer has one, try it on a round test part first.
2. Tune pressure advance
Pressure advance (called linear advance in Marlin) tells the printer to push a little extra plastic when it speeds up and pull back a little when it slows down. That cancels most of the lag that causes corner bulges and thin line starts.
- On Prusa printers the command is M572 for the MK4/S, XL, MINI and CORE One, and M900 for the MK3.
- In Marlin the command is M900, for example M900 K0.08.
- On Klipper you run a pressure advance test and read the best value from the printed corners. The PrintPal wiki gives example values for the test: square corner velocity 1, acceleration 500 and a factor of 0.005, or 0.020 for long Bowden setups. Typical results fall in a range of about 0.05 to 1.0, with the high values mostly on Bowden extruders.
Many Bambu Lab and other modern printers tune this for you in the calibration menu of the slicer. If your printer offers an automatic flow dynamics or pressure advance calibration, run it for each filament type. Different filaments need different values.
The PrintPal wiki gives a clear order for tuning: calibrate the temperature first, because hotter plastic oozes more, then pressure advance, then retraction. If you tune retraction first and pressure advance later, you may have to redo the retraction.
3. Check retraction
Retraction pulls the filament back before the nozzle travels, so plastic does not leak. Too little leaves strings and zits at the start of each move. Too much can leave gaps and a thin start to the next line.
- Make sure retraction is turned on.
- Use your slicer's profile for your printer and filament as the starting point, then change one value at a time. The retraction settings guide shows how to test length and speed with a small tower.
- Turn on wipe while retracting if your slicer has it. The nozzle then moves a short distance along the wall as it retracts, which cleans the tip. Cura calls this the outer wall wipe distance.
- Avoid travelling across visible walls. A slicer option that avoids crossing perimeters keeps travel moves inside the part, where they are hidden.
Coasting, which stops extruding just before the end of a loop, is an option in some slicers. In Cura it is marked experimental, and the PrintPal wiki notes that Marlin recommends turning coasting off once linear advance works. Treat it as a last step, not a first one.
4. Lower the temperature a little
If your filament oozes, a slightly lower nozzle temperature reduces the amount of plastic that leaks during moves. Stay inside the range printed on the spool, and go down in steps of 5 °C. A temperature tower shows you where the surface is cleanest for that spool.
5. Look at flow and moisture
If the whole surface is lumpy, not only the seam, try these two checks:
- Over-extrusion makes every line a little too thick, and the extra plastic piles up in corners and at the seam. A small reduction in the flow ratio often clears it. The flow rate calibration guide explains how to measure the right value.
- Wet filament boils inside the nozzle and leaves bubbles, a rough finish and small pops while printing. If you hear popping, dry the spool before you change any other setting. The filament drying guide covers temperatures and times.
6. Slow down the outer wall
Printing outer walls at a moderate speed helps because there is less pressure change between straight sections and corners. Many slicers let you set the outer wall speed on its own, so you can leave infill fast and slow only the surface that shows.
A short test routine
Use one small cylinder or a calibration cube and change one thing per print.
- Set the seam to Aligned or Rear and print. Note where the line ends up.
- Turn on scarf seams, if your slicer offers them, and print again.
- Run the pressure advance calibration for the filament and apply the result.
- Adjust retraction and wipe only if bumps are still spread around the walls.
- Lower the temperature by 5 °C if there is still ooze.
Keep each printed test and write the setting on it with a marker. After four or five prints you will see which change made the most difference.
When it is not the settings
If you have tried everything above and still see bumps in the same place, look at the hardware. A partly clogged nozzle gives uneven flow, and a worn or loose extruder gear can make pressure inconsistent. See the guides for a clogged nozzle and for under-extrusion if the surface also has gaps.
Frequently asked questions
What is the difference between a blob and a zit?
In everyday use the words mean nearly the same thing: a small bump on the surface. Some people use blob for a larger lump, often at a corner, and zit for a small bump. The causes and fixes overlap.
Where is the best place for the seam?
For most parts, the back or the least visible side. On boxy parts, a sharp corner hides it well. On round parts there is no corner, so use Aligned or Rear and turn the part so the seam faces away from you.
Can I remove zits after printing?
Yes. Small bumps can be shaved with a hobby knife and sanded. PLA and PETG both sand, although PETG can gum up the paper. For a smooth finish on a visible part, fix the settings first, because the effort of sanding repeats on every print.
Will pressure advance fix all blobs?
No. It fixes bulges at corners and thin line starts, which are caused by pressure lag. It does not fix moisture, over-extrusion or a damaged nozzle. Use it together with the seam and retraction checks above.
Does a bigger nozzle make blobs worse?
A larger nozzle holds more pressurised plastic, so pressure effects can be stronger and seams more visible. The same fixes apply, but you may need to tune pressure advance again for the new nozzle.